452 XXXI International Mineral Processing Congress 2024 Proceedings/Washington, DC/Sep 29–Oct 3
Table 1. Ore sorter conditions and parameters used for dynamic tests with the lithium ore sample
Test ID Feed
Color DE-XRT
%area* RD† %area‡
E7 37.0 kg of –4.0/+1.5 rocks 60−230 60−100
E11 31.5 kg of –4.0/+1.5 rocks 25−100
E15a 18.0 kg of –1.5/+0.5 rocks 119−230 24−100
E15b 15.5 kg of –1.5/+0.5 rocks 20−100
*The %area parameter of the color sensor is in the range of 0% to 100%, and it was used to specify the percent area of pixels over
the surface of a particle that must have the (greenish) white color corresponding to that of spodumene grains visible on some rocks.
RD =relative density. The RD parameter is in the range of 0 (least dense) to 230 (most dense).
The %area parameter of the DE-XRT sensor is in the range of 0% to 100%, and it was used to specify the percent area of pixels
over the surface of a particle that must have a pixel density of the value specified by the RD parameter.
Table 2. Conditions and parameters of production tests with
size fractions of the lithium ore sample
Separation Run No.
Color
%area*
1 45−100
2 25−100
3 5−100
*%area parameter of color sensor as defined in Table 1.
Figure 3. Processing scheme used for production tests with size fractions of the lithium ore sample