XXXI International Mineral Processing Congress 2024 Proceedings/Washington, DC/Sep 29–Oct 3 451
Figure 2. Results of dynamic tests with color (a, b, c, d) and DE-XRT (e, f, g, h) sensors on –4.0/+1.5 and –1.5/+0.5 size
fractions of the lithium ore sample