XXXI International Mineral Processing Congress 2024 Proceedings/Washington, DC/Sep 29–Oct 3 1949
Figure 11. Effect of collector dosage on floatation froth carbon and iron recovery for –25 micron BFD
Figure 12. Effect of collector dosage on floatation froth yield for three different sizes