Figure 1. Change of floatation results with grinding fineness (pulp pH 9.3, depressor
addition 0.5 kg/t tails feed, collector addition 1.2 kg/t tails feed)
Figure 2. Change of flotation results with pH of pulp (grinding fineness 52.70 wt% of
–200 mesh particles, depressor addition 0.5 kg/t tails feed, collector addition 1.2 kg/t
tails feed)
Figure 1. Change of floatation results with grinding fineness (pulp pH 9.3, depressor
addition 0.5 kg/t tails feed, collector addition 1.2 kg/t tails feed)
Figure 2. Change of flotation results with pH of pulp (grinding fineness 52.70 wt% of
–200 mesh particles, depressor addition 0.5 kg/t tails feed, collector addition 1.2 kg/t
tails feed)